Table 2 chemical composition of major oxides (in wt.%)

From: Chemical, mineralogical and physical study of Late Iron Age ceramics from Nditam: Cameroon (West central Africa)

Samples

Group

SiO2

Al2O3

Fe2O3

MnO

MgO

CaO

Na2O

K2O

TiO2

P2O5

LOI

CNDI 01

3

55.66

20.63

11.27

0.04

2.04

0.79

0.18

1.62

1.54

0.22

5.57

CNDI 02

3

53.21

23.35

11.44

0.08

1.58

0.82

0.56

3.91

2.27

0.21

1.89

CNDI 03

2

57.90

25.47

6.18

0.03

0.88

1.07

0.70

1.38

1.32

0.28

4.09

CNDI 04

2

56.77

25.91

7.29

0.03

1.95

1.83

0.79

1.34

0.79

0.37

2.15

CNDI 05

1

62.11

20.96

3.92

0.03

1.01

0.97

0.59

1.59

0.92

0.88

6.40

CNDI 06

3

63.88

18.39

6.30

0.05

1.25

0.69

0.13

3.36

1.84

0.31

3.11

CNDI 07

2

63.19

24.89

3.08

0.01

0.43

0.83

0.50

2.65

0.77

0.13

2.78

CNDI 08

2

66.25

20.70

3.76

0.03

0.65

0.64

0.15

2.12

2.20

0.19

2.57

CNDI 09

3

57.86

19.89

10.93

0.05

1.95

0.89

0.23

2.54

1.74

0.30

2.93

CNDI 10

2

62.76

19.64

9.10

0.03

1.44

0.78

0.22

1.43

1.30

0.30

2.57

CNDI 11

2

64.49

21.17

3.93

0.03

0.77

0.83

0.69

3.15

1.07

0.21

2.89

CNDI 12

2

58.07

25.41

6.20

0.02

0.68

0.89

0.12

2.82

1.65

0.33

3.02

CNDI 13

2

68.62

15.91

6.06

0.03

1.56

0.4

0.07

2.17

1.02

0.23

3.44

  1. LOI stands for loss on ignition