Fig. 4From: Investigation of coloured lead glass glitter from an early eighteenth century material collection, Cambridge, by electron microscopy/energy dispersive X-ray analysisSEM image of cross-section from I/34, a brown (above) and golden flake, EDX spots are marked in white. Insert light microscopy not to scaleBack to article page