From: Hydrating softwood and hardwood samples using pure and modified supercritical carbon dioxide

Fig. 11

OH/“Cellulose” peak areas (around 3460 and 4020 cm−1 respectively) in DRIFT spectra obtained for Maple (blue), White Oak (red), Zebrano (green) and Red Oak (magenta) having undergone the five different treatments: oven-dried, 2.5 mol% MeOH, 5.0 mol% MeOH, 10.0 mol% MeOH and soaked. Each bar represents the overall mean from calculated ratio areas ± one standard error of the mean