Table 2 A table to show oven-dried wood samples in decreasing order of mean strength prior to treatment with scCO2(PURE) and scCO2(MeOH)

From: Hydrating softwood and hardwood samples using pure and modified supercritical carbon dioxide

Wood species

MOR of samples (MPa)

Wood type

Zebrano (M)

791

Tropical hardwood

Keruing (H)

718

Maple (M)

640

Hardwood

Maple (H)

634

White Oak (M)

528

Red Oak (M)

519

White Oak (H)

514

Scots Pine (H)

110

Softwood

  1. Strength values have been stated to an accuracy of 3 significant figures