Fig. 5From: Oak wood degradation processes induced by the burial environment in the archaeological site of Biskupin (Poland)Pyrolytic profile of the sound oak wood reference sample. Holocellulose (H) and lignin (L) pyrolysis products are indicatedBack to article page