Fig. 10From: Corrosion of glaze in the marine environment: study on the green-glazed pottery from the Southern Song “Nanhai I” shipwreck (1127–1279 A.D.)Scatter plot of component distribution in pristine glaze, inner and outer Si-rich layers (Data from Table 1-N4; Additional file 1: Table S2-EDX6, EDX7; Additional file 1: Table S5-EDX2, EDX5)Back to article page