Skip to main content

Table 2 The integral area ratios of the bending envelope to stretching envelope in the Raman spectra of the pristine glaze and the Si-rich layer (A470/A950) and the peak positions and integral area ratios of each component (Qn) in the stretching envelope (AQn/A950)

From: Corrosion of glaze in the marine environment: study on the green-glazed pottery from the Southern Song “Nanhai I” shipwreck (1127–1279 A.D.)

Regions

A470/A950

Parameters

Q0

Q1

Q2

Q3

Q4

Pristine glaze

0.18

Peak position

859

902

960

1001

AQn/A950

0.07

0.34

0.48

0.11

Si-rich layer

0.56

Peak position

855

900

955

995

1130

AQn/A950

0.07

0.23

0.26

0.26

0.20