Skip to main content

Table 5 SEM–EDS analysis results of different internal (I) and external (II) corrosion layers of two  copper samples (wt.%)

From: Atmospheric corrosion in the metal pool of Ali Qapu palace in Isfahan: an experimental study

Sample

Cu

O

Cl

Pb

As

Sn

Sb

Ag

S

Fe

Al

Zn

Bi

AQ-01

I

88.38

7.31

0.13

–

0.42

0.55

0.58

0.37

0.19

0.42

0.35

0.81

0.49

I

68.95

21.41

0.28

1.9

0.61

0.74

1.43

0.88

0.17

0.79

0.23

2.64

–

II

64.25

22.98

1.52

–

0.53

5.65

0.32

0.41

1.36

0.37

–

1.97

–

AQ-02

I

80.01

12.06

1.04

–

–

5.04

0.21

0.14

–

0.29

–

1.21

–

I

80.01

16.76

0.1

–

–

1.95

–

0.24

–

0.2

–

0.74

–

I

69.32

18.18

9.31

–

–

0.41

0.79

0.43

0.46

0.29

0.12

0.69

–

II

34.54

31.19

0.28

1.61

0.59

29.4

–

0.36

–

0.47

0.75

0.81

–

II

26.21

2.72

0.33

–

0.33

67.98

–

0.58

0.18

0.29

 

0.53

0.85