Skip to main content

Table 7 Ecor and icor values evaluated from potentiodynamic polarizations curves after 7 days of immersion in NaCl 0.1M

From: Corrosion of aircraft heritage: a comparison between modern and historic Duralumin alloys

 

Ecor (mV/SCE)

Jcor (A/cm2)

EBD (mV/SCE)

Rolled

B(p)

− 0.722

2.34 × 10–6

− 0.592

2024(p)

− 0.722

1.44 × 10–6

− 0.550

2017A(p)

− 0.75

1.46 × 10–6

− 0.524

Extruded

B(s)

− 0.757

1.43 × 10–6

− 0.584

2024(s)

− 0.757

1.43 × 10–6

− 0.584